3M 890
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- High-Strength Filament Reinforcement
- Heavy-Duty Bundling Support
- Industrial Splicing and Securing
Product Description
Scotch Filament Tape 890 is a high-strength glass-filament reinforced polyester tape for heavy-duty bundling, reinforcing, splicing, and securing. Its reinforced construction is used where grouped materials require a high-strength tape wrap during industrial handling, packaging, or transport. The same product supports heavy-duty splicing and component-securing work without changing tape type. The product is intended for heavy-duty industrial packaging and handling tasks. It is available in multiple widths and roll lengths for different roll-format requirements.
Key features
- High-strength filament reinforcement: Glass-filament reinforced construction provides the strength needed for demanding bundling and securing tasks.
- Heavy-duty bundling use: The tape is used to bundle pipes, rods, conduit, and timber during industrial handling.
- Industrial splicing and securing: The product supports heavy-duty paper splicing and secures appliance and furniture lift flaps.
Applications
Scotch Filament Tape 890 is used for heavy-duty bundling of pipes, rods, conduit, and timber, heavy-duty paper splicing, and securing appliance and furniture lift flaps.