3M 898
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- High-Tensile Filament Reinforcement
- Multi-Surface Synthetic-Rubber Adhesion
- Consistent Curl-Resistant Dispensing
Product Description
Scotch Filament Tape 898 is a clear filament-reinforced polypropylene tape with a multi-layer synthetic-rubber adhesive system for high-strength reinforcement and heavy-duty strapping. The 0.168 mm construction combines glass yarn filaments with a backing that resists nicks, abrasion, moisture, scuffing, and breakage, even when nicked or punctured. Its adhesive bonds to corrugated cardboard, fiberboard, plastics, metals, and oily surfaces, and the tape is engineered to dispense consistently without curling. The reinforced construction is intended for demanding packaging, shipment reinforcement, bundling, and strapping work.
Key features
- High-tensile filament reinforcement: Glass yarn reinforcement provides long-term holding power and high tensile strength for demanding packaging loads.
- Multi-surface synthetic-rubber adhesion: The adhesive system bonds to corrugated cardboard, fiberboard, plastics, metals, and oily surfaces.
- Durable controlled dispensing: The reinforced backing resists abrasion and moisture while the roll dispenses consistently without curling.
Applications
Applications include full-overlap L-clip box closures, metal and pipe bundling, large bulk-container reinforcement, high-strength reinforcement, and heavy-duty strapping.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Backing | Polypropylene film | Clear filament-reinforced construction | |
| Fiber reinforcement | Glass yarn | As supplied | |
| Adhesive system | Multi-layer synthetic rubber | Pressure-sensitive | |
| Total tape thickness | 0.168 | mm | Typical |
| Product color | Transparent | As supplied |